Heat Treatment of Paulownia tomentosa Steud. Wood
Keywords:
Density, Absorption, Brinell hardness, Mechanical properties, Tensile strength parallel to the grain, Thickness swellingAbstract
Heat treatment of Paulownia tomentosa wood was studied relative to the physical and mechanical properties, with a view to expanding the potential fields of use of this species. Several physical properties (density, water absorption after 2 and 24 h, thickness swelling) and mechanical ones (strength and modulus of elasticity in static bending, tensile strength parallel to the gran and Brinell hardness) were evaluated. Most physical and mechanical properties of Paulownia wood were superior in the radial direction, with the exception of tensile strength, regardless of whether the samples were subjected to torrefaction treatment or not. In addition, the water affinity of heat-treated wood decreased significantly, with water absorption after 2 h of immersion reduced by 21% and tangential thickness swelling after 2 h of immersion reduced by 36.6%. The static flexural modulus of elasticity decreased by 12.1% at temperature of 160 ºC treatment, by 39.9% for the 180 ºC treatment and by 52.8% for the at temperature of 20 ºC treatment.