Effect of Borate Treatment on Mechanical and Fire Properties of Cross-laminated Timber Manufactured from Poplar and Spruce
Keywords:
Cross-laminated timber, Fire retardancy, Borate, Poplar, Spruce, Modulus of elasticity, Bending strengthAbstract
Effects of a 12% borate solution treatment on the mechanical properties and fire resistance of three-layer cross-laminated timber (CLT) panels were evaluated for poplar (Populus alba) and spruce (Picea abies) woods. Mechanical testing (modulus of elasticity (MOE), modulus of rupture (MOR)) followed ANSI/APA PRG 320 (2018), and fire performance was assessed via ASTM E69 (2014). The borate treatment did not cause statistically significant changes in the MOE or MOR of poplar (p > 0.10); however, for spruce, a statistically significant reduction was observed in both MOE (14.5% reduction, p = 0.08) and MOR (31.3% reduction, p = 0.05) at the 90% confidence level. Inherent mechanical properties differed significantly, with poplar CLT exhibiting higher MOE and MOR than spruce. In contrast, the borate treatment significantly improved fire resistance by increasing the time to ignition) 43 to 62% increase) and reducing mass loss (14 to 30% reduction) for both species. Spruce CLT demonstrated higher inherent fire resistance than poplar in both treated and untreated states. The findings indicated that borate treatment effectively enhanced the fire performance of CLT without compromising its mechanical integrity. Consequently, borate-treated poplar CLT presents a viable material for non-structural applications requiring fire resistance, offering the potential to reduce reliance on imported softwoods.