Abrasive Wear Performance of Tropical Hardwoods Under Two-Body Contact

Authors

  • Aubin Takoudjou talla Laboratory of Mechanics and Modeling of Physical Systems (L2MSP), Faculty of Science, University of Dschang, Dschang, West Cameroon https://orcid.org/0000-0003-3539-9800
  • Rene Ngouffo Koukougnang Higher Technical Teachers’ Training College (HTTTC), Department of Mechanical Engineering, University of Buea, Kumba, Cameroon; Department of Mechanical and Industrial Engineering, Faculty of Engineering and Technology, University of Buea, Buea, Cameroun https://orcid.org/0000-0001-9123-5152
  • Ulrich Gael Azeufack Tonfack Department of Mechanical and Industrial Engineering, Faculty of Engineering and Technology, University of Buea, Buea, Cameroun
  • Claude Takoumbe Higher Technical Teachers’ Training College (HTTTC), Department of Mechanical Engineering, University of Buea, Kumba, Cameroon https://orcid.org/0000-0003-3968-7551
  • Lie Regis Moumbina Laboratory of Mechanics and Modeling of Physical Systems (L2MSP), Faculty of Science, University of Dschang, Dschang, West Cameroon
  • Sandrine Mabekou Laboratory of Mechanics and Modeling of Physical Systems (L2MSP), Faculty of Science, University of Dschang, Dschang, West Cameroon
  • Pierre Kisito Talla Laboratory of Mechanics and Modeling of Physical Systems (L2MSP), Faculty of Science, University of Dschang, Dschang, West Cameroon

Keywords:

Wear coefficient, Tropical hardwoods, Sliding abrasion, Sliding speed, Tribological behavior, Surface degradation

Abstract

Abrasive wear behavior was studied for three tropical hardwood species, Tieghemella heckelii (makore), Khaya anthotheca (mahogany), and Pericopsis elata (assamela), under various normal loads and sliding speeds. Two-body abrasion tests were performed perpendicular to the grain, dry and without lubrication, at sliding speeds of 20 to 70 rpm and under normal loads of 250, 500, and 750 g. The wear coefficient (k) was determined from the slope of the quasi-linear steady-state portion of the wear volume and sliding distance relationship. All species exhibited an initial running-in phase followed by a steady-state wear regime. Makore displayed the lowest average wear coefficients, while assamela exhibited the highest values. Increasing the load from 250 to 500 g reduced the wear coefficient by 32.9% to 36.3%, while the reduction between 500 and 750 g was more moderate (10.1% to 17.5%), indicating a non-linear load dependence. This behavior could be related to variations in actual contact conditions and deformation of the wood’s cellular structure. Sliding speed induced a non-monotonic, species-dependent response, with critical speed ranges corresponding to minimum and maximum wear coefficients. Overall, the results demonstrate that resistance to abrasive wear depends on the combined effects of wood species, normal load, and sliding speed. These results provide useful guidance for selecting tropical hardwoods for applications involving abrasive mechanical contact.

Downloads

Published

2026-09-30

How to Cite

Takoudjou talla, A., Ngouffo Koukougnang, R., Azeufack Tonfack, U. G., Takoumbe, C., Moumbina, L. R., Mabekou , S., & Talla, P. K. (2026). Abrasive Wear Performance of Tropical Hardwoods Under Two-Body Contact. BioResources, 21(4), 11211–11227. Retrieved from https://ojs.bioresources.com/index.php/BRJ/article/view/25064

Issue

Section

Research Article or Brief Communication